EVATANE® 33-15 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-15 is stabilized with antioxidants. The High Vinyl Acetate content of EVATANE® 33-15 brings softness, flexibility and polarity. EVATANE® 33-15 delivers high cohesive strength with any kind of fillers (HFFR compounds).Information provided by Arkema Group |