MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake Elevate™ EF545AW 4.0% EVA copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: EF545AW resin is a 4.0% VA ethylene vinyl acetate copolymer with high antiblock designed for stretch and other film applications where cold temperature performance and low C.O.F. are needed. This grade provides reasonable optics even with the high antiblock loading necessary to achieve the low C.O.F. Excellent cold temperature performance, toughness, and resistance to load deformation make EF545AW a wise selection for wrapping pallets stored in food freezers and other cold environments. Test specimens for blown film: nominal thickness 1.5 mils; blow up ratio 2.4:1, die gap 35 mils. This product has some 21 CFR clearances. Application/Uses: Pallet wrap stretch film- Food packaging stretch film.

Samples tested at 23°C and 50% RH.

Information provided by Westlake Chemical Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.931 g/ccASTM D1505
Thickness 1.50 milBlown Film as Tested
Melt Index of Compound 0.55 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 225 %ASTM D882
Film Elongation at Break, TD 600 %ASTM D882
Coefficient of Friction 0.50ASTM D1894
Dart Drop 107 g/mil
@Thickness 0.0381 mm
ASTM D1709
Dart Drop Test 160 g
@Thickness 0.0381 mm
ASTM D1709
Film Tensile Strength at Break, MD 3320 psiASTM D882
Film Tensile Strength at Break, TD 2550 psiASTM D882
1% Secant Modulus, MD 25000 psiASTM D882
1% Secant Modulus, TD 30000 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 13 %ASTM D1003
Gloss 50 %45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Die Opening 0.0350 inBlown Film as Tested
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene
Versalis Clearflex® H&T CLH 196 Hexene Copolymer Linear Low Density Polyethylene
Versalis Clearflex® H&T CLH 150 Linear Low Density Polyethylene
Versalis Clearflex® H&T CLH 108 Octene Copolymer Linear Low Density Polyethylene

PWESF8811 / 222883

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.