MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Spraycore® SC 4055 Mold Building Compound
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: SC 4055 is a ceramic compounded vinyl ester/polyester resin blend that was formulated for the production of fiberglass molds. This product will enhance the cosmetic appearance, rigidity and speed of production of fiberglass reinforced molds. MEEK is not included. Preferred red dye catalyst: HP-90, DHD-9, MEEK 925. Product features: minimizes fiberglass print through in the production of fiberglass molds, reduces the amount of entrapped air behind the gel coat, helps to reduce the transfer of the fiberglass pattern onto the tooling gel coat, helps make parts stronger and more rigid. Product benefits: can be used as a core and a tooling gel coat, helps speed up production due to fast cure times and low shrinkage, offers user friendly application.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.70 - 10.7 lb/galApplication density
Viscosity 8000 - 11000 cPRVF #5 @ 20rpm
 
Chemical PropertiesOriginal ValueComments
Styrene Content 26 %
 
Processing PropertiesOriginal ValueComments
Gel Time 0.500 - 1.50 minwith MEKP 925 Catalyst
 5.00 - 10.0 minGel to Peak with MEKP 925 Catalyst
 5.00 - 15.0 minGel to Peak with HP-90 Catalyst
 8.00 - 13.0 minwith HP-90 Catalyst
 
Descriptive Properties
Colorblack
Peak Exotherm275 to 305°F100g mass with HP-90 Catalyst
 300 to 350°F100g mass with MEKP 925 Catalyst

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWS9054 / 239564

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.