MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® MonoPlus MK 51 Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus MK 51 is a styrene-based, monodispersed, macroporous weak base anion exchanger with polyhydroxy groups showing a very high selectivity for the removal of boric acid or borates from water. The high selectivity of borate to the resin allows a separation of boric acid from water and aqueous electrolyte solutions also a high salt concentration. Lewatit MonoPlus MK 51 can especially be used for:
  • the removal of boron from waste water or contaminated ground water
  • the removal of boron from RO permeate in purpose to produce water for irrigation
  • the removal of boron traces in the production of ultrapure water or chemicals
  • removal of boron from high concentrated magnesium chloride solution
  • adsorption of oxoanions of W, Mo, V Ge, As, Sb, from processes streams
The resin is appropriately exhausted at a specific flow rate of 10…20 BV/h. The regeneration can be done with hydrochloric or sulfuric acid. To reach high capacity levels it is recommended to make a two stage regeneration using a sodium hydroxide solution for the second treatment (conditioning).

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.670 g/cc
Density 1.14 g/cc
Bead Size 0.500 - 0.600 mmMean
Storage Temperature -20.0 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 50.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sodium Tetraborate, Na2B4O7
Sodium Tetraborate Tetrahydrate, Na2B4O7-4H2O
Sodium Tetraborate Pentahydrate, Na2B4O7-5H2O
Sodium Tetraborate Decahydrate, Na2B4O7-10H2O
Sodium Metasilicate, Na2SiO3

PLANY8785 / 209177

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.