Excellent cold workability. Fabricated by extrusion, drawing, heading, impacting, machining. Applications: resistance welding electrodes, circuit breakers, feed-through conductors, heat sinks, motor parts, high-strength high-temperature parts. Test specimen: rod - 16mm diameter; 56% cold worked.Inactive per the Copper Development Association. |