MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Röchling Polystone® G Virgin Natural HDPE/PE300
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes:
  • Excellent overall mechanical properties
  • Easy to machine and weld
  • High chemical resistance
Product applications:
  • Tanks & Vessels
  • Food cutting boards
  • Light-duty guides & rails

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccASTM D792
Water Absorption <= 0.10 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength, Yield 4000 psiASTM D638
Elongation at Break >= 700 %ASTM D638
Tensile Modulus 217000 psiASTM D638
Flexural Modulus 210000 psiASTM D790
Izod Impact, Notched 3.50 ft-lb/inASTM D4020
Coefficient of Friction, Dynamic 0.20 - 0.29
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+14 ohmASTM D257
Dielectric Constant 2.4
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µin/in-°FASTM D696
Melting Point 268 °F
Maximum Service Temperature, Air 180 °F
Deflection Temperature at 1.8 MPa (264 psi) 165 °FASTM D648
Brittleness Temperature <= -103 °FASTM D746
Flammability, UL94 HB
@Thickness 3.17 mm
 
Compliance PropertiesOriginal ValueComments
FDA Yes
NSF No
USDA Yes
 
Descriptive Properties
ColorOpaque White; Blue-FDA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GEHR Plastics PET Polyethylene Terephthalate
RTP Company RTP 799 X 143519 U EG High Molecular Weight Polyethylene (HMWPE), ESD Protection - Permanently Static Dissipative - UV Stabilized
RTP Company RTP 799 X 143519 B EG High Molecular Weight Polyethylene (HMWPE), ESD Protection - Permanently Anti-static - Extrusion Grade - Preliminary Datasheet
Röchling Polystone® D HMW (PE-500) High molecular weight PE
DuPont Teijin Films Mylar® RB52 Polyester Film, 50 Gauge

PROCH9018 / 232722

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.