MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Permabond ES578 Epoxy Resin
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: PERMABOND® ES578 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces, ceramics as well as composite materials. ES578 provides excellent thermal conductivity and bond strength. ES578 was designed for application requiring heat dissipation such as bonding aluminum heat sinks to ceramic headers.

The cured adhesive has been designed to meet the fire retardancy requirements of UL94 V-0.

Features & Benefits:

  • Very good thermal conductivity
  • Excellent resistance to vibration
  • Easy to use – no mixing required
  • High shear and peel strength
  • High temperature resistance
  • Good resistance to chemicals
  • Designed to meet the requirements of UL94

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.55 g/ccUncured
Viscosity 600000 - 800000 cP
@Temperature 25.0 °C
Uncured
Storage Temperature 2.00 - 7.00 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 84
Adhesive Bond Strength 14.0 - 27.0 MPaZinc, Shear; ASTM D1002
 17.0 - 31.0 MPaAluminum, Shear; ASTM D1002
 27.0 - 41.0 MPaSteel, Shear; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 µm/m-°C
Thermal Conductivity 1.30 W/m-K
 
Processing PropertiesOriginal ValueComments
Cure Time <= 180 secInduction
 0.500 hour
@Temperature 150 °C
Oven
 1.00 hour
@Temperature 130 °C
Oven
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceBlackUncured
Maximum Gap Fill (mm)5
Strength Retention100% at 0°CRelative to 0°C
 25% at 200°CRelative to 0°C
 65% at 150°CRelative to 0°C
 85% at 100°CRelative to 0°C
 95% at 50°CRelative to 0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® 3872 1 component acrylic/urethane UV/Heat Cure Flexible Adhesive
Hexcel® HexPly® F593 Epoxy Resin
Solvay CYCOM® 7714 Epoxy Resin
Atom Adhesives AA-BOND 2110 Epoxy Adhesive
Armstrong A-7 Epoxy Adhesive

PPERMA899 / 162772

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.