MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
BASF Ultramid® 8202 HS BK-102 PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Ultramid 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose injection molding PA6 exhibiting excellent fluidity for filling thin sections. It possesses the combination of strength, stiffness and toughness properties as well as excellent chemical, thermal and abrasion resistance. The heat stabilizer system extends its retention of properties at elevated temperatures.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccdry; ISO 1183
Water Absorption 1.6 %24 hour; ISO Test
 9.5 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 2.7 %beginning dry (23°C/50% R.H.); ISO 62
Relative Viscosity 2.6 cPISO Test; 96 % SAV
Viscosity Measurement 48Formic Acid
Linear Mold Shrinkage 0.012 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 36.0 MPa50mm/min; ISO 527
 36.0 MPa2 in/min; ASTM Test
Elongation at Break >= 50 %50mm/min, Nominal strain; ISO 527
 >= 100 %2 in/min; ASTM Test
Elongation at Yield 16 %50mm/min; ISO 527
 16 %2 in/min; ASTM Test
Tensile Modulus 970 MPa1mm/min; ISO 527
Flexural Strength 25.0 MPaISO Data
 35.0 MPaASTM Test
Flexural Modulus 770 MPaISO Data
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10 K/min
 220 °CASTM Test
 
Descriptive Properties
ColorBK-102
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicHeat stabilized or stable to heat
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8202 HS BK-102 PA6 (Dry)
BASF Ultramid® 8200 HS PA 6 (Conditioned)
BASF Ultramid® 8202 PA6 (Conditioned)
BASF Ultramid® 8202C PA6 (Conditioned)
BASF Ultramid® 8202 PA6 (Dry)

PBASF9142 / 84906

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.