MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Matexcel BIOD-011 PCL Granule
Categories: Wood and Natural Products

Material Notes: BIOD-011; PCL Granule; biodegradable material; Biopolymer materials

Application: Drug release: The degradation rate of PCL is slower than that of other biodegradable polyesters, and it can be prepared into various forms such as microspheres, microcapsules, nanospheres and nanofibers through microfluidic, electrospinning and other technologies for long-term use. drug delivery systems; Tissue engineering: The melting point of PCL is as low as about 60°C, and it can be used to print hearts and other tissue engineering scaffolds in the medical field; Medical equipment: PCL has good thermoplasticity and molding processability, and can be made into fibers, sheets, sheets, etc. by extrusion, blow molding and injection molding, etc., which can be used as surgical sutures, medical equipment, etc.; Cell culture: PCL can be used as a skeleton component of cell culture microcarriers;

Morphology: White Powder

Key Words: Synonyms: PCL Granule
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 4.00 °C
 
Descriptive Properties
Product overviewThis product is a granular e-caprolactone homopolymer (PCL), which meets the GMP standard in the pharmaceutical field and can be directly used in the production of medical devices or pharmaceutical preparations.
Viscosity0.2 dl/g; 0.4 dl/g; 0.8dl/g; 1.2 dl/g; 1.7 dl/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK1981 / 300612

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.