Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping, offering unique aspect and cost reduction advantage. Availability: Africa & Middle East, Asia Pacific and Europe Key Features: - Low sealing threshold
- High seal strength even under low pressure sealing
- Excellent packaging machine performance
- Outstanding optical properties
- No seal compatibility between acrylic coating and coex film
- Water-based coatings
Features:- Acrylic Coated
- Flavor & Aroma Barrier
- In Lamination Lap Sealable
Applications: Uses: - Tobacco Overwrap Flexible Packaging
Processing Method: Solvent Flexographic Printing, Solvent Rotogravure Printing and Surface Print UnsupportedInformation provided by ExxonMobil |