MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Aperam Resistohm® 145 Resistant Alloys Iron-Chromium-Aluminium Alloys
Categories: Metal; Ferrous Metal

Material Notes: Resistohm 145 is a ferritic alloy of the FeCrAl family, which can be used up to 1300°C in case of big diameters. To maintain Resistohm 145 under 1000°C during 7 to 8 hours in an oxidizing atmosphere with an unsufficient quantity of oxygen or air induces formation of a white-grey aluminum coat of oxyde which protects the wire of a possible chemical attack. It is recommended to oxyde the wire of this way when the element must operate in reducting conditions. This is why Resistohm 145 is generally supplied preoxidised. Resistohm 145 can be used for resistances in electric furnaces for ceramic, chemical and metallurgic industries, and for all applications where it is necessary to apply very high temperature of use. Life time of Resistohm 145 is better than those of NiCr in case of atmospheres containing sulfur and particularly if they are oxidizing. Life time of Resistohm 145 is particularly influenced by the formation of oxide coat. If the atmosphere does not permit it, life time in high temperatures is considerably reduced. Prejudicial atmospheres are nitrogen, ammonia, and hydrocarbons.

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.10 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 230
Tensile Strength 750 MPa
Tensile Strength, Yield 550 MPa
Elongation at Break >= 18 %on 100 mm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000145 ohm-cmTemperature coefficient = 0.000033/°C from 20 - 100°C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 16.0 W/m-K
@Temperature 120 °C
Melting Point 1500 °C
Maximum Service Temperature, Air 1300 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 6.0 %
Chromium, Cr 23 %
Iron, Fe 71 %
 
Descriptive Properties
Creeping point1.5at 1000°C
 8at 800°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aperam Resistohm® 125 Resistant Alloys Iron-Chromium-Aluminium Alloys
330 Stainless Steel
Outokumpu 4845 High Temperature Austenitic Stainless Steel
AISI 1006 Steel, cold drawn
AISI 1005 Steel

NPERA089 / 194878

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.