Premi-Glas® 2103-25 CR-SX is a 25% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:- Underwriters Laboratories, U.L. 94-V0 flame recognition at 2.54mm minimum wall thickness.
- U.L. recognized in all colors.
- Available in glass contents ranging from 10% - 30%; standard product has 22% reinforcement.
- Excellent dielectric strength, arc and track resistance.
- Chemical resistant and self-extinguishing properties.
- Designed for Compression, Transfer and Injection molding processes.
Data provided by Premix. A. Schulman has acquired this former Premix product line. |