MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Matexcel NAT-195 Gellan Gum HAP
Categories: Other Engineering Material

Material Notes: Loss on drying(%) =15.0 Lead(mg/kg) =2.0 Particle size(%) 80 Mesh =98 Suspension Test Pass Ash(%) =15 PH(0.5% Solution) 5.0—7.0 Bacterium account(CFU/g) =10000 Coliforms(MPN/100g) =30 Yeast and mould(CFU/g) =400 Salmonella 0/25g

Application: HAP Type Gellan gum is a kind of high acyl gellan gum. It is manufactured by fermentation from a carbohydrate source(glucose). High Acyl Gellan gum is in natural organization without deacylation.The organization of Gellan Gum HAP is a premium quality refined tan / white powder. Gellan Gum HAP is specialized high acyl Gellan Gum for applicatin in acid or netural plant protein based beverage.

Morphology: White to Tan powder

Uses: 1.Dispersion:Gellan Gum HAP can be dispersible readily into plant protein beverage systems using regular mixing devices.The product can be activated by heating treatment such as UHT, HTST, pasteurization and retort procession. 2. Dissolution:Gellan Gum HAP is improved by heating treatment (time, temperature),shear stress (stirrer, homogenizer). A complete dissolution can be easily obtained at around 85?-90? for 20-30minutes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Purity>85.0%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK1253 / 299884

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.