MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Palm Labs Adhesives Turbo Fuse Series 115SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115SI – SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performance has been tested with a variety of materials, and is recommended for a multitude of applications. The fast curing qualities make it especially desirable in high speed industrial production. TURBO FUSE SERIES 115SI is ideal for use in applications that require an easily handled low viscosity adhesive on difficult surfaces. Because of the 20 viscosity, it works especially well in close to medium fitting applications that have difficult bonding surfaces.

Part Numbers for this data: 04-115SI, 10-115SI, 15-115SI, 20-115SI, 25-115SI, 30-115SI, 35-115SI

Soluble in Acetone, MEK, Amide, Methylene Chloride

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 123-31-9
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 20 cPLiquid State
 
Mechanical PropertiesOriginal ValueComments
Shear Strength >= 1450 psiASTM D1002/DIN 53283
 >= 1740 psiASTM D1002/DIN 53283
 >= 2610 psiASTM D1002/DIN 53283
 >= 2900 psiASTM D1002/DIN 53283
 >= 3190 psiASTM D1002/DIN 53283
 2610 - 4060 psiTensile, (Cured State)
 >= 3630 psiASTM D1002/DIN 53283
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 - 170 °CCured State
Maximum Service Temperature, Air 180 °FCured State
Minimum Service Temperature, Air -60.0 °FCured State
Flash Point 160 - 200 °FLiquid State (Tag closed cup)
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourFull, Cured State
Shelf Life 12.0 MonthLiquid State
 
Descriptive Properties
AppearanceClear liquidLiquid State
 Clear-HardCured State
Base compound (Resin)Surface Insensitive Ethyl CyanoacrylateLiquid State
Gap Fill0.05 mmCured State
Material Set Up Time<3 secRubber
 12-18 secCeramics
 1-5 secWood
 2-5 secPlastics
 5-15 secLeather
 8-10 secMetals

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPALML014 / 135168

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.