MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phosphor bronze 8% Sn, UNS C52100, HR06 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: Extra Hard and Stress Relieved

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Butt Weld; Good Suitability – Gas Shielded Arc Welding, Spot Weld, Capacity for Being Cold Worked; Fair Suitability – Oxyacetylene Welding, Coated Metal Arc Welding, Seam Weld; Poor Suitability – Capacity for Being Hot Formed

Common Fabrication Processes: Blanking; Drawing; Forming and Bending; Shearing; Stamping

Typical uses: Bridge Bearing Plates; Thermostat Bellows; Coinage; Power Conductor for Electro-Surgical Pencil; Cold Headed Parts; Electrical Connectors; Electrical Flexing Contact Blades; Electronic Connectors; Fuse Clips; Switch Parts; Wire Brushes; Cotter Pins; Fasteners, Heavy Duty; Lock Washers; Beater Bar; Bellows; Bourdon Tubing; Chemical hardware; Clips, Heavy Duty; Clutch Disks; Cold Headed Parts; Diaphragms; Doctor Blades, Paper Industry; Gears; Perforated Sheets; Pinions; Pneumatic Hammers; Sleeve Bushings; Springs, Heavy Duty; Springs, Helical Extension; Springs, Helical Torsion; Textile machinery; Thrust Bearings; Truss Wire; Welding Wire; Well Drill Equipment; Marine Parts

Applicable Specifications: Bar – ASTM B139/B139M, ASTM B103/B103M; Electrode – Welding AWS A5.6, Welding MILITARY MIL-E-23765/3; Plate – ASTM B103/B103M; Rod – Welding AWS A5.15, ASTM B139/B139M; Shapes – ASTM B139/B139M; Sheet – ASTM B103/B103M, SAE J463, SAE J461; Strip – ASTM B888/B88M; SAE J463, ASTM B103/B103M, SAE J461; Wire – ASTM B159/B159M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.318 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 105 ksi
Tensile Strength, Yield 93.0 ksi0.2% Offset
Elongation at Break 15 %
Tensile Modulus 16000 ksi
Modulus of Rigidity 6000 ksi
Poissons Ratio 0.33Calculated
Machinability 20 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000132 ohm-cm13% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.1 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 36.0 BTU-in/hr-ft²-°F
Melting Point 1620 - 1880 °F
Solidus 1620 °F
Liquidus 1880 °F
Annealing Point 900 - 1250 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 90.3 - 93 %As Balance
Iron, Fe <= 0.10 %
Lead, Pb <= 0.050 %
Phosphorus, P 0.030 - 0.35 %
Tin, Sn 7.0 - 9.0 %
Zinc, Zn <= 0.20 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC52100x2 / 293002

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.