MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gabriel Versamid® 140 Polyamide Resin
Categories: Polymer; Thermoset

Material Notes: Versamid® products have proven to be superior coatings resins in many applications, such as industrial maintenance and marine coatings, high-performance architectural paints and high-solids and conventional coatings.

Advantages:

  • Highly resistant to chemical and water corrosion
  • Strong adhesion to a variety of substrates
  • Long pot life
  • Lower sensitivity to substrate impurities
  • Most comply with FDA regulations
Principal Applications: Coatings, castings, potting, laminating and adhesives

Comments/Advantages: Moderately low-viscosity, excellent chemical resistance

Information provided by Gabriel Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 lb/gal
Solids Content 100 %Theo
Viscosity 8000 - 12000 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 6400 psiAfter 7 days 25°C cure
Elongation at Break 3.8 %After 7 days 25°C cure
Flexural Strength 13600 psiAfter 7 days 25°C cure
Flexural Modulus 326000 psiAfter 7 days 25°C cure
Compressive Strength 11400 psiAfter 7 days 25°C cure
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg <= 93.0 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 8.0
 
Processing PropertiesOriginal ValueComments
Cure Time 390 minTack Free Time; 3 wet mils
 720 minThrough Cure; 3 wet mils
Pot Life 210 min60% solids
Gel Time 135 min200 mg Mass
 
Descriptive Properties
Amine Value370-400[mg KOH/g]
Chemical Resistance to 10% Acetic Acid11.58% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to 10% H4SO41.29% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to 10% HCl0.92% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to 10% NAOH0.47% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to Ethanol5.36% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to MEKDES% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to Xylene13.36% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical TypePolyamide
PHR for Max DSC, Tg51190 EEW Epoxy
Theo Amine Hydrogen Equl Wt.97

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGABR979 / 230680

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.