MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Corning Polarcor™ Glass Polarizer, 800 nm Nominal Wavelength
Categories: Ceramic; Glass; Optical

Material Notes: Polarcor™ is used as an optical element in polarization-dependent isolators, optical modulators, polarimetry systems, ellipsometers, shutters and other polarization-based devices. Polarcor is characterized by high extinction and low insertion loss throughout the 600 nm to 2300 nm wavelengths (depending on grade). Polarcor is a borosilicate glass that contains titanium, aluminum and silver. The polarizing mechanism is elongated silver crystals in the outer 20 µm ? 50 µm of the glass surface; this ensures the elimination of stray light, by absorbing the unwanted polarization. Since Polarcor is a solid glass product it is extremely resistant to chemical, physical and thermal damage, while exhibiting excellent optical properties.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.412 g/cc
Thickness 500 microns
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 480kg/mm2
Modulus of Elasticity 58.6 GPa
Poissons Ratio 0.21
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.50 µm/m-°C
Specific Heat Capacity 0.770 J/g-°Cestimated by Corning
Thermal Conductivity 0.00240 cal cm/sec-cm²-°C
@Temperature 1.00 °C
 0.00270 cal cm/sec-cm²-°C
@Temperature 100 °C
 0.00300 cal cm/sec-cm²-°C
@Temperature 200 °C
 0.00330 cal cm/sec-cm²-°C
@Temperature 300 °C
 0.00350 cal cm/sec-cm²-°C
@Temperature 400 °C
 0.00380 cal cm/sec-cm²-°C
@Temperature 500 °C
 0.00430 cal cm/sec-cm²-°C
@Temperature 600 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.5161
@Wavelength 800 nm
Abbe Number 57.6
Transmission, Visible >= 84 %
@Wavelength 740 - 860 nm
Insertion Loss without AR-Coating < 0.76 dB
 >= 91.3 %
@Wavelength 740 - 860 nm
Insertion Loss for 2 sides AR-Coated < 0.39 dB
Reflection Coefficient, Visible (0-1) <= 0.0040Reflectance R per each side
 
Descriptive Properties
Brewster's Angle56.3°
Contrast>10,000:1Extinction Ration > 40 dB
Polarization Bandwidth (nm)740 - 860

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CCORNG921 / 282892

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.