MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® HL5505 Blow Molding HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Extra High Molecular Weight Copolymer

Applications: 55 gallon drums (even those with demanding built-in handling rings), industrial tanks

Formolene HL5505 is intended for large part blow molding applications. Besides having excellent chemical resistance properties HL5505 HDPE has outstanding environmental stress crack resistance properties, and exceptional impact and creep resistance.

Formolene HL5505 meets all requirements of ASTM D1248 - Type II, Category 5.

Formolene HL5505 meets all requirements of ASTM - Type III, Category 5 and ASTM 4967-89-PE235.

Produced using licensor formulation for HXM TR-570. Licensor does not warrant or imply that this product meets their specifications for HXM TR-570.

Nominal properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928. Physical properties are typical of product but do not reflect normal testing variance and therefore should not be used for specification purposes.

Information provided by Formosa Plastics Corporation, USA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccASTM D1505
ESCR 100% Igepal® >= 1000 hourCondition A, F50; ASTM D1693
ESCR 10% Igepal® >= 1000 hourCondition B, F50; ASTM D1693
High Load Melt Index 5.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4000 psi2" (50mm) per min.; ASTM D638 Type IV
Elongation at Break >= 600 %2" (50mm) per min.; ASTM D638 Type IV
Flexural Modulus 195000 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -119 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Petromont 1000 High Density Polyethylene Resin
Formosa Plastics Formolene® DB5305A Blow Molding HDPE
Chevron Phillips Marlex® HXB TR-512 Extra high molecular weight polyethylene
Chevron Phillips Marlex® C516 HDPE Blow Molding Resin

PFPCPE16 / 38823

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.