MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin SF2250EPR Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: 20% Glass fiber filled, super high flow polyetherimide(PEI) (TG 217degC) with internal mold release and balance properties with flow and ductility, ECO conforming, UL94 V0 listing.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant,High Flow

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D792
Density 1.4314 g/ccISO 1183
Water Absorption 0.136 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
 0.0500 %23°C/50% RH/24 hrs; ISO 62-4
Viscosity 12 cP
@Load 2.16 kg,
Temperature 360 °C
MVR cc/10 min; ISO 1133
 21 cP
@Load 6.70 kg,
Temperature 337 °C
MVR cc/10 min; ISO 1133
 57 cP
@Load 10.0 kg,
Temperature 345 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.003833 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.004466 cm/cmSABIC method
Melt Flow 12.9 g/10 min
@Load 2.16 kg,
Temperature 360 °C
ASTM D1238
 21.9 g/10 min
@Load 6.70 kg,
Temperature 337 °C
ASTM D1238
 56 g/10 min
@Load 10.0 kg,
Temperature 345 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 136 MPa5 mm/min; ISO 527
 145 MPa5 mm/min; ASTM D638
Elongation at Break 2.3 %5 mm/min; ISO 527
 2.5 %5 mm/min; ASTM D638
Tensile Modulus 8747 MPa1 mm/min; ISO 527
 9057 MPa5 mm/min; ASTM D638
Flexural Strength 197 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
 199 MPabreak, 2mm/min; ISO 178
 201 MPayield, 2 mm/min; ISO 178
 202 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 7619 MPa2 mm/min; ISO 178
 7796 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 79.7 JASTM D256
Izod Impact, Unnotched 368 J/mASTM D4812
Izod Impact, Notched (ISO) 8.80 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²80*10*4; ISO 180/1U
Charpy Impact Unnotched 35.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 8.50 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
 23.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
CTE, linear, Transverse to Flow 54.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
 70.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 209 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 205 °C
@Thickness 6.40 mm
unannealed; ASTM D648
 207 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 203 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 198 °C
@Thickness 6.40 mm
unannealed; ASTM D648
 201 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 210 °CRate B/50; ISO 306
 211 °CRate B/120; ISO 306
 212 °CRate B/50; ASTM D1525
 213 °CRate B/120; ASTM D1525
UL RTI, Electrical 105 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 105 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.50 - 1.60 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 345 - 400 °C
Zone 2 345 - 400 °C
Zone 3 345 - 400 °C
Melt Temperature 350 - 400 °CInjection Molding
Mold Temperature 135 - 165 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82757 / 290704

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.