MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Domo TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.

Available in: Asia Pacific

Product Applications: TECHNYL C 218 MZ20 V10 offers an excellent planarity of the end product, high mechanical properties and a high dimensional stability. This grade is commonly used in the automotive industry to mould large parts with a low warpage, such as: car body parts, engine covers, housings.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183/A
Linear Mold Shrinkage 0.0057 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0054 cm/cm
Linear Mold Shrinkage, Transverse 0.0095 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPaISO 527 Type 1A
Elongation at Break 3.3 %ISO 527 Type 1A
Tensile Modulus 7400 MPaISO 527 Type 1A
Flexural Strength 255 MPaISO 178
Flexural Modulus 9300 MPaISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²ISO 180/1eA
Izod Impact, Unnotched (ISO) 82.0 kJ/m²ISO 180/1eU
Charpy Impact Unnotched 60.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 14.1 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75/Af
 
Processing PropertiesOriginal ValueComments
Feed Temperature 230 - 235 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone235-240°C
Mixing Zone240-250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B3ZG6 BK30564 30% Glass Filled PA6 (Dry)
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry)
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry)
BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Dry)

PRHOD765 / 137996

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.