Function: Ultra-accelerator of natural and synthetic rubber vulcanization; vulcanizing agent for vulcanization without free sulfur or for low-sulfur vulcanization Application: Technical rubber articles of all kinds, heat-resistant technical articles, e.g. cable sheathing and insulation, hard rubber Information provided by Lanxess. |