MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
AK Steel ASTM A 424 Type II, VIT-PLUS® DS Enameling Carbon Steel
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: VIT-PLUS is a controlled chemistry, non-decarburized steel designed to replace certain types of ingot products. It has good strength after fire properties. It is not recommended for direct-on cover coat porcelain enamel applications. VIT-PLUS is free of fishscale regardless of the enamel

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 311 MPa.0275 - .035 inches sheet thickness; ASTM A 370
Tensile Strength, Yield 198 MPa.0275 - .035 inches sheet thickness; ASTM A 370
Elongation at Break 43 %in 2 inches; ASTM A 370
Modulus of Elasticity 200 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000142 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.4 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.481 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 89.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.050 %
Carbon, C 0.040 %
Copper, Cu 0.020 %
Iron, Fe 99.65 %As Remainder
Manganese, Mn 0.21 %
Phosphorus, P 0.010 %
Silicon, Si 0.010 %
Sulfur, S 0.010 %
 
Descriptive Properties
Deep-Drawing Capability rm1.3.0275 - .035 inches sheet thickness
Strain Hardening Exponent n0.21.0275 - .035 inches sheet thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel ASTM A 424 Type 1, UNIVIT® DS Enameling Carbon Steel
AK Steel ASTM A 424 Type III, I-F Enamel Enameling Carbon Steel
AK Steel ASTM A 568 and A 635 Hot Rolled Carbon Steel, Structural Steel (SS)
ASTM A36 Steel, plate
AK Steel NITRONIC® 19-D Duplex Stainless Steel

NAKS087 / 14690

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.