MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® 4502 Adhesive
Categories: Polymer; Adhesive

Material Notes: Product Description: LOCTITE® Product 4502 is a low viscosity, fast curing, single component cyanoacrylate adhesive. It is specifically formulated for difficult to bond substrates.

Typical Applications: Rapid bonding of a wide range of metal, plastic or elastomeric materials, particularly suited for bonding porous or absorbent materials such as wood, paper, leather or fabric

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Viscosity 70 - 130 cP
@Shear Rate 3000 1/s
MK-22 Cone
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 0.300 - 0.600 MPaNitrile rubber; ASTM D1002
 0.700 - 0.800 MPaNeoprene rubber; ASTM D1002
 4.10 - 5.30 MPaZinc dichromate; ASTM D1002
 7.10 - 11.8 MPaPhenolic; ASTM D4501
 15.4 - 17.5 MPaGrit Blasted Aluminum; ASTM D1002
 10.1 - 27.9 MPaPVC; ASTM D4501
 18.4 - 20.4 MPaGrit Blasted Steel; ASTM D1002
 24.9 - 29.4 MPaPolycarbonate; ASTM D4501
 26.8 - 30.8 MPaABS; ASTM D4501
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Surface Resistance 1.90e+16 ohmASTM D257
Dielectric Constant 3.1
@Frequency 1000 Hz
ASTM D150
 3.2
@Frequency 10000 Hz
ASTM D150
Dielectric Strength 780 V/milASTM D149
Dissipation Factor 0.028
@Frequency 1000 Hz
ASTM D150
 0.028
@Frequency 10000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696
Glass Transition Temp, Tg 127 °CASTM E228
Flash Point >= 93.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT5081 / 255292

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.