MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Mallard Creek Polymers Rovene® 4181 Carboxylated Styrene-Butadiene Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Rovene 4181 is a styrene-butadiene emulsion that can be compounded to high solids using calcium carbonate, clays and alumina trihydrate as fillers. Rovene 4181 imparts good wet/dry tensile strength, and has good adhesion to a wide variety of surfaces. Rovene 4181 is a low VOC containing latex that is crosslinkable with external crosslinkers.

Markets: Paints and Coatings

Applications: Wood Coating, Metal Coating

Related Products: Rovene 4546, Rovene 4180, Rovene 6026, Rovene 6121

Information provided by Mallard Creek Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 54.5 - 55.5 %
pH 7.0 - 7.5
Viscosity <= 1500 cP
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 14.0 °C
 
Descriptive Properties
Minimum Film Formation Temperature (°C)18.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMCP9922 / 250424

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.