Hexene Copolymer Linear Medium Density Polyethylene for foaming applications. It is formulated for inner layers with excellent foam cell structure and smooth surface finish and uniform closed cells. It increases thickness, durability, impact resistance and stiffness of molded part. Meets CONEG regulation for articles intended for direct food contact. Information provided by Polimeros Mexicanos |