MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Borealis Borlink™ LE0310-04 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Borlink LE0310-04 is a crosslinkable black polyethylene compound, specially designed for semiconductive strippable insulation shield of power cables.

Applications: Borlink LE0310-04 is indented for semiconductive strippable insulation shield in medium voltage (MV) AC cables with rated voltages up to 46 kV. The values are voltages between phases as defined in ICEA S-94-649.

Specifications: Borlink LE0310-04 is expected to meet the applicable requirements included in the below mentioned standards provided it is processed using sound material handling, extrusion and crosslinking practices as well as appropriate testing procedures. This applies up to the maximum recommended voltage level indicated in "Applications" section above since some standards cover wider voltage ranges. IEC 60502-2; AEIC CS8; ANSI/ICEA S-93-639; ANSI/ICEA S-94-649; ANSI/ICEA S-97-682; UL 1072

Special Features: Borlink LE0310-04 is a ready-to-use semiconductive compound. It provides very low strip forces when used over Borealis crosslinkable polyethylene insulation compounds. The excellent distribution of carbon black and additives in Borlink LE0310-04 results in a smooth semiconductive shield.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccASTM D792
Storage Temperature 10.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 11.2 MPa20 in/min; ASTM D638
 8.40 MPa
@Treatment Temp. 121 °C,
Time 605000 sec
retained after temperature exposure; ASTM D638
Elongation at Break 300 %20 in/min; ASTM D638
 300 %
@Treatment Temp. 212 °C,
Time 605000 sec
ASTM D638
Peel Strength 10.0 pli5 lbs/½ inch Cable Strip Force (90° peel)
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 50.0 ohm-cm
@Temperature 23.0 °C
ASTM D 991
 <= 500 ohm-cm
@Temperature 90.0 °C
ASTM D 991
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -40.0 °CASTM D 746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 115 - 125 °C
Shelf Life 24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9646 / 323003

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.