Data provided by Solvay Engineered Polymers. A thermoplastic olefinic elastomer (TPO) designed for exterior automotive applications requiring excellent low-temperature toughness. This material exhibits durable paintability with flexible automotive enamels and improved resistance to marring. Uses: Sight shields, fender flares, bumper end caps, and other applications requiring exacting dimensional tolerances. LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line. |
Thermoplastic Olefinic Elastomer; Polyolefin |