MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Petropol Tenopom® B3 P15 S2 NTLA016 PR341 POM, PTFE Filled, Conditioned
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, PTFE Filled

Material Notes: Product Description: High Flow, Polyacetal Copolymer

Resin ID (ISO 1043): POM-S
Additive: PTFE, Silicone
Processing: Injection Molding, Extrusion
Color: Natural, Opaque

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccASTM D792
Water Absorption 0.20 %
@Temperature 50.0 °C,
Time 86400 sec
Immersion; ASTM D570
Linear Mold Shrinkage 0.015 - 0.018 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110ASTM D785
Tensile Strength 31.0 MPa
@Temperature 80.0 °C
ASTM D638
 37.0 MPa
@Temperature 60.0 °C
ASTM D638
 48.0 MPa
@Temperature 23.0 °C
ASTM D638
 69.0 MPa
@Temperature -40.0 °C
ASTM D638
Elongation at Break 25 %
@Temperature -40.0 °C
ASTM D638
 28 %
@Temperature 23.0 °C
ASTM D638
 64 %
@Temperature 60.0 °C
ASTM D638
 99 %
@Temperature 80.0 °C
ASTM D638
Modulus of Elasticity 0.590 GPa
@Temperature 80.0 °C
ASTM D790
 1.00 GPa
@Temperature 60.0 °C
ASTM D790
 1.85 GPa
@Temperature 23.0 °C
ASTM D790
 3.50 GPa
@Temperature -40.0 °C
ASTM D790
Tensile Modulus 680 MPa
@Temperature 80.0 °C
ASTM D638
 950 MPa
@Temperature 60.0 °C
ASTM D638
 1950 MPa
@Temperature 23.0 °C
ASTM D638
 2900 MPa
@Temperature -40.0 °C
ASTM D638
Flexural Modulus 2800 MPaASTM D790
Izod Impact, Notched 70.0 J/mASTM D256
Izod Impact, Unnotched 690 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 170 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 215 °CMolding
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time 3.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPETROPOL379 / 313287

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.