HexPly® 920 is a very tough advanced resin matrix, ideally suited to the single-shot production of honeycomb sandwich structures and the manufacture of solid laminates. It is highly tolerant of a variety of production techniques and equipments, making it easy to process. The high toughness of HexPly® 920 makes it ideal for industrial applications and performance cars. it is available preimpregnated into carbon, glass or aramid fibers.Information provided by HexCel |