MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M 4314 Single-Coated Foam Tape
Categories: Polymer; Tape

Material Notes: 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plasticized) as tape adhesion is typically satisfactory within 20 minutes and continues to build and additional time.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0320 g/ccfoam with adhesive; ASTM D3574
Thickness 3.00 milRelease Liner
 250 milTotal
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 8.0Foam with adhesive; ASTM D2240
Tensile Strength at Break 0.170 MPaDie "A"; ASTM D3759
Elongation at Break 125 %Die "A"; ASTM D3759
Compressive Strength 0.300 psiDeflection, Compress 25%; ASTM D3574
Compression Set 5.0 %ASTM D1667
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 2.00e+12 ohmNon-adhesive side; ASTM D257
 6.00e+12 ohmAdhesive side; ASTM D257
Dielectric Strength 40.0 kV/inASTM D149
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0430 W/m-KASTM C518
 
Descriptive Properties
Adhesive Type430
AppearanceCharcol gray
 Tanliner

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM34560 / 169307

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.