Product Description: A biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. Typically, all gauges are used laminated with other substrates on HFFS and VFFS applications. 30MM480 can be used as single web mainly on HFFS packaging machines. Availability: Africa & Middle East, Asia Pacific and Europe Key Features: - Excellent adhesion of aluminum to film
- Excellent moisture barrier
- Excellent light barrier
- Good hot tack
- High yield
- Easy to convert
- Brilliant metal appearance
Features:- In Lamination Lap Sealable
- Light Barrier
- Moisture Barrier
Applications:- Bakery
- Biscuits/Cookie/Crackers
- Confectionery, Chocolate
- Confectionery, Gum
- Confectionery, Sugar
- Crisps and Snacks
- Frozen Food
- Ice Cream
- Pet Food
Uses: - HFFS Flexible Packaging
- Pre-made Bags – Flexible Packaging
- VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Surface Print UnsupportedInformation provided by ExxonMobil |