MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRILOY™ Compound Z2000 Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: LNP LUBRILOY Z2000 compound is based on Polyphenylene Ether / Polystyrene (PPE/PS) blend containing proprietary lubricant. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
 1.04 g/ccISO 1183
Moisture Absorption 0.0600 %23°C/50% RH/24 hrs; ASTM D570
 0.0700 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0089 cm/cm24hrs; ASTM D955
 0.0089 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0115 cm/cm24hrs; ASTM D955
 0.0115 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 41.0 MPaISO 527
 42.0 MPaASTM D638
Tensile Strength, Yield 38.0 MPaISO 527
 46.0 MPaASTM D638
Elongation at Break 37.3 %ISO 527
 52.3 %ASTM D638
Elongation at Yield 3.2 %ISO 527
 4.2 %ASTM D638
Tensile Modulus 1810 MPa1 mm/min; ISO 527
 1820 MPa50 mm/min; ASTM D638
Flexural Strength 58.0 MPaISO 178
 74.0 MPaASTM D790
Flexural Modulus 1860 MPaISO 178
 2080 MPaASTM D790
Izod Impact Notched 106 JASTM D256
Izod Impact, Unnotched 2034 J/mASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 172 kJ/m²80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.19ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.24ASTM D3702 Modified: Manual
K (wear) Factor 121 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 81.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 82.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 88.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 89.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 138 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 140 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 121 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 260 - 270 °C
Zone 3 265 - 275 °C
Melt Temperature 275 - 295 °CInjection Molding
Mold Temperature 60.0 - 95.0 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81159 / 289106

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.