MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-TA-77 TPU for Shoe Adhesive
Categories: Polymer; Adhesive

Material Notes: Product Description:
  • Excellent initial bonding strength
  • good solvent solubility
  • strong crystallization
  • low thermoplasticity
Advantages:
  • Excellent initial bonding strength
  • good solvent solubility
  • strong crystallization
  • low thermoplasticity
  • mono-component adhesive
  • cross-linking agent
Applications: Excellent bonding strength for TPU, PVC, Nylon, Polyester, fabrics, leather. Suitable for shoes, textile industry and fire hose co-extrusion.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1600 - 1800 cP15% in MEK
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 - 15.0 minTack time (PVC// PVC)
 
Descriptive Properties
Activation Temperature55-65°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN744 / 267052

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.