MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound D351RCC Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP D351RCC compound is based on recycled Polycarbonate (PC) resin containing 30% glass fiber. Added features of this grade include: High Modulus, Low Warpage, Good Ductility, Non-Brominated & Non-Chlorinated Flame Retardant. Post-Consumer Recycling (PCR) Polycarbonate content up to 40%.

Features: Post-Consumer Recycled (PCR) content,High Stiffness,Enhanced Ductility,Flame Retardant,Non-Chlorinated,Non-Brominated,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.425 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
Viscosity 31 cP
@Load 2.16 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0010 - 0.0030 cm/cm24hrs; ASTM D955
Melt Flow 19 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 36 g/10 min
@Load 2.16 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 127 MPa5 mm/min; ISO 527
 130 MPa5 mm/min; ASTM D638
Elongation at Break 2.4 %5 mm/min; ASTM D638
 2.7 %5 mm/min; ISO 527
Tensile Modulus 9210 MPa5 mm/min; ASTM D638
 9400 MPa1 mm/min; ISO 527
Flexural Strength 183 MPa2 mm/min; ISO 178
 195 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 7810 MPa2 mm/min; ISO 178
 8550 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 130 JASTM D256
Izod Impact, Unnotched 465 J/mASTM D4812
Izod Impact, Notched (ISO) 13.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 31.0 kJ/m²80*10*4; ISO 180/1U
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 118 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 113 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 122 °CRate B/50; ISO 306
 126 °CRate B/120; ISO 306
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.800 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 285 - 305 °C
Zone 2 270 - 290 °C
Zone 3 280 - 300 °C
Melt Temperature 285 - 310 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 110 °CInjection Molding
Dry Time 3.00 - 6.00 hourInjection Molding
Back Pressure 0.100 - 0.300 MPa
Screw Speed 50 - 90 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81487 / 289434

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.