MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® G-310HBP Fluoroelastomer Copolymer, 66% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-310HBP is a medium viscosity bisphenol curable, gum copolymer. It has excellent mold flow for transfer or compression molding. Properly compounded, DAI-EL® G-310HBP produces vulcanizates with excellent heat and compression set resistance.

Typical Applications: O-rings, Shaft seals, gaskets, molded tubing

Rheological Properties MDR 2000:
Temperature: 177°C
Frequency: 100 cpm
Strain: 0.5°
Test time: 6 min

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.81 g/cc
Mooney Viscosity 47
@Temperature 121 °C
ML 1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 77
Tensile Strength at Break 15.8 MPa
Elongation at Break 210 %
100% Modulus 6.20 MPa
@Strain 100 %
Compression Set 13 %
@Temperature 200 °C,
Time 252000 sec
#214 O-ring; ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -18.0 °CLow Temperature Retraction; ASTM D1329
 
Processing PropertiesOriginal ValueComments
Cure Time 0.900 mints2, scorch time
 1.10 mint'50, time to 50% cure
 1.70 mint'90, time to 90% cure
 10.0 min
@Temperature 177 °C
Press Cure
 24.0 hour
@Temperature 232 °C
Post Cure
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 66 %
 
Descriptive Properties
ColorBeige to pale brown
MH24.4 dNmmaximum torque
ML1.5 dNmminimum torque
Test Formula0.5 phrPhosphonium accelerator
 100 phrDAI-EL® G-310HBP
 2 phrBisphenol AF
 3 phrMagnesium oxide
 30 phrMT Carbon Black (N-990)
 6 phrCalcium hydroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDAIJ9814 / 209885

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.