MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Jushi E7 Glass Fiber
Categories: Ceramic; Glass

Material Notes: Compared to traditional E Glass, E7 has 30% higher strength, 23% higher modulus, and a higher softening point. It offers better corrosion resistance than B-free E glass in acid, alkaline, and neutral aqueous solutions.

Information provided by Jushi Group Co. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.58 g/ccASTM D1505
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 89.0 GPaSonic Method
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 7.0
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.51 µm/m-°CASTM D696
Softening Point 921 °CASTM C338
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.562Oil Immersion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Jushi E7 568H Chopped Glass Strands
C.O.I.M. FILCO® 354 N Unsaturated Bisphenolic Polyester Polymer for Glass Fiber Sizing
Jushi E7 DR-386T Direct Roving - Polyester Composite
Jushi UD1200 Glass Fiber Epoxy Composite
Borealis Himod™ FT7324 LDPE for Film

EJUSHI990 / 183360

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.