DANTHANE_ 126K-Powder is a polyester based, TPU-powder for transparent coatings. DANTHANE_ 126K-Powder is used for different powder sinter coatings. Furthermore this TPU is also suitable for laminations of different materials. It can also be used for thermoplastic adhesion equipments, for example for label material that will be applied later by thermobatch sealing process. Application: DANTHANE_ 126K-Powder can be used at the coating as intermediate layer and final coating. This powder is best suitable for the lamination of textiles with supporting films by flat film lamination applications. This medium-hard TPU is mainly used for the coating of transport and conveyer belts as well as for flat belt material and flexible materials for containers. DANTHANE_ 126KPowder can also be combined with other DANADD_ powders in different colours. This can be used as intermediate layer and then as top coat DANTHANE_ 126K-Powder will be applied. Information provided by Danquinsa GMBH |