MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Veriva® VR-501 Polyphenylsulfone (PPSU), Biomaterial
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Veriva® VR-500 and VR-501 are grades of polyphenylsulfone (PPSU) offered for use in implantable devices. Veriva® VR-500 is the neat version of the polymer and Veriva® VR-501 is an opaque white grade.

The manufacturing facility for Veriva® PPSU in Alpharetta, GA is ISO 13485 registered and the relevant aspects of current Good Manufacturing Practices are also applied.

Our biomaterials manufacturing processes are carefully validated and enhanced controls provide product traceability. In addition, all materials are tested in a lab that is ISO 17025 accredited.

An FDA MAF is available.

Applications: Body Implants; Medical/Healthcare Applications

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 - 1.33 g/ccASTM D792
Melt Flow 13 - 20 g/10 min
@Load 5.00 kg,
Temperature 365 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 68.9 MPaASTM D638
Elongation at Break >= 6.5 %ASTM D638
Tensile Modulus >= 1900 MPaASTM D638
Izod Impact, Notched >= 530 J/mASTM D256
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
Cytotoxicity - ISO 10993:5Pass
FormsPellets
Physiochemical Testing - ISO 10993:18Pass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4615 / 280415

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.