MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ravago Manufacturing Americas Hylex® P1032L Polycarbonate, Unreinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.

Information provided by Entec.

Key Words: Highest Flow, Mold Release
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Water Absorption 0.15 %24-Hr Immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 32 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80ASTM D785
Tensile Strength, Yield 9700 psiASTM D638
Elongation at Break 120 %ASTM D638
Flexural Strength 12500 psiASTM D790
Flexural Modulus 300000 psiASTM D790
Izod Impact, Notched 12.0 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 1.85 ft-lb/in
@Thickness 3.17 mm,
Temperature -30.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 4.00e+16 ohm-cmASTM D257
Dielectric Strength 406 V/mil
@Thickness 3.17 mm
in Air; ASTM D149
Arc Resistance 120 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 132 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °CASTM D648
Vicat Softening Point 305 °FASTM D1525
Flammability, UL94 V-2
@Thickness 1.50 mm
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.585ASTM D542
Haze 0.50 - 0.80 %
@Thickness 3.17 mm
ASTM D1003
Transmission, Visible 89 - 91 %
@Thickness 3.17 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Entec Hylex® P1010L2 HB Polycarbonate
Entec Hylex® P1325L1 HB Polycarbonate
Entec Hylex® P1017L2 HB Polycarbonate
Entec Hylex® P1007L1 HB Polycarbonate
Entec Hylex® P1010L1 HB Polycarbonate

PENT051C / 36079

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.