MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Indium Corp. WF-9955 Wave Solder Flux, Halogen-Free
Categories: Fluid; Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: WF-9955 soldering flux is an updated version of WF-9942, designed to conform to the more rigorous standards of J-STD-004B Type ORL0. It has no intentionally added halogens, no rosin, and exhibits exceptional hole fill as well as pin-testing performance that can only be achieved with a rosin-free material. In addition to exhibiting excellent soldering performance on a wide range of board finishes and board types, WF-9955 also passes the updated and more rigorous reliability requirements of the J-STD-004B Surface Insulation Resistance (SIR) and Electromigration (ECM) tests.

Information provided by Indium Corporation.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.796 g/cc
@Temperature 25.0 °C
 0.803 g/cc
@Temperature 15.0 °C
Solids Content 4.71 %
 
Chemical PropertiesOriginal ValueComments
Acid Value 26.25mgKOH/g flux
 557.24mgKOH/g flux solids
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+8 ohmIPC-TM-650
 
Thermal PropertiesOriginal ValueComments
Flash Point 54.0 °FTCC
 
Processing PropertiesOriginal ValueComments
Shelf Life 48.0 Month
@Temperature <=40.0 °C
unopened container

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NNIN995c / 197393

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.