Applications:- Basic raw material of silicon oil (modified silicon oil), silicon emulsion, silicon rubber, silicon resin etc. organic products
- treatment agent for rubber filler
- Raw material of cosmetic
- Thermal plastic rubber and thermal setting additive
- Various engineering plastics
- Release agent
Information provided by Go Yen Chemical |