MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DSM Arnite® TV4 260SF TV4 260 SF PBT (EU and Asia)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: 30% Glass Fiber Reinforced, Flame Retardant, High Flow

Processing Notes (See more info below): Screw Speed: Medium . Injection Speed: Slow-Medium.

Information provided by DSM Engineering Plastics.

Artnite is a former DSM Engineering Plastics product line now with Envalior, although this specific product was discontinued prior to that transaction

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.64 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %ISO 62; at 50% RH
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm2 mm thickness; ISO 2577
 0.0050 - 0.0090 cm/cm4 mm thickness; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 130 MPaISO 527
Elongation at Break 2.5 %ISO 527
Modulus of Elasticity 11.0 GPaISO 527
Flexural Strength 190 MPaISO 178
Flexural Modulus 9.50 GPaISO 178
Izod Impact, Notched (ISO) 7.50 kJ/m²ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75
Flammability, UL94 V-00.75 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 238 - 249 °C
Middle Barrel Temperature 243 - 266 °C
Front Barrel Temperature 249 - 260 °C
Nozzle Temperature 243 - 254 °C
Melt Temperature 249 - 266 °C
Mold Temperature 60.0 - 88.0 °C
Drying Temperature 250 °Fto 0.02% for molding
Dry Time 2 - 4 hourdesiccant hopper dryer preferred

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSM166 / 30847

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.