MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® GE120 Electrically and Thermally Insulating Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Material Description: A single component, thixotropic, electrically and thermally insulating epoxy adhesive designed for bonding SMDs to the PCB. It can be used for electronic assembly in many devices including consumer electronics, cell phone, telecommunications, medical, automotive, and scientific/OEM. It is a blue color version of EPO-TEK® 115-SMT.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/cc
Particle Size <= 20 µm
Viscosity 200000 - 300000 cP
@Temperature 23.0 °C
1 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80
Tensile Modulus 439000 psiStorage
Shear Strength 1568 psiLap
 >= 1700 psiDie
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 7.00e+13 ohm-cm
Dielectric Constant 3.18
@Frequency 1000 Hz
Dissipation Factor 0.0070
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 41.0 µm/m-°CBelow Tg
 218 µm/m-°CAbove Tg
Maximum Service Temperature, Air 175 °CContinuous
 275 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 65.0 °CDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 344 °CDegradation Temperature
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Temperature 150 °C
minimum
 15.0 min
@Temperature 120 °C
minimum
Pot Life 40320 min
Shelf Life 1.00 Month
@Temperature 23.0 °C
 12.0 Month
@Temperature -40.0 °C
 
Descriptive Properties
ColorBluebefore cure
ConsistencySmooth Thixotropic paste
Number of ComponentsSingle
Weight Loss0.27%200°C
 1.12%250°C
 2.96%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® OE120 Two Component Epoxy

PPOXYT159 / 141198

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.