MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay MACKINE® 401 Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Mackine 401 is slightly soluble in water but becomes readily soluble when neutralized with acid, becoming a cationic surfactant. The tertiary amine group can also react with hydrogen peroxide, chloroacetate and aklylchlorides to form amine oxides, betaines and quaternary ammonium compounds. As a cationic surfactant, Mackine 401 becomes substantive to hair and provides conditioning properties. The degree of conditioning depends on the types of acid used. Lactic, citric and propionic acids have been found to be excellent choices. In addition, the salts formed with Mackine 401 are compatible with anionic surfactants and will not depress foam. This enables the development chemist to incorporate Mackine 401 into conditioning shampoos without introducing the negative effects found with quaternary ammonium compounds. Provides a very soft feel.

INCI Name: Isostearamidopropyl Dimethylamine

CAS: 67799-04-6

EINECS: 267-101-1

Uses: Liquid Conditioners, Cream Rinses and Cream Hair Conditioners

Information provided by Rhodia, Rhodia has been acquired by Solvay. The Mackine® brand has been sold to Verdant Specialty Solutions, although this specific grade has been discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.870 g/cc
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 6.0
 
Processing PropertiesOriginal ValueComments
Shelf Life 48.0 Month
 
Descriptive Properties
AppearanceClear to Hazy Liquid
CompositionAmidoamine>90% MW=376
 Amine Number150-165
 DMAPA<1%
 Free Fatty Acid<4% MW=294

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WRHOD226 / 137457

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.