MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Nilcra® Zirconia 3Y-TZP Grade Y-TZP
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Yttria-Tetragonal Zirconia Polycrystal (Y-TZP) with excellent transformation toughening properties. Comprising 3 mol% (5.2 wt%) Y2O3 in ZrO2. A high purity, fine grain (sub-micron) tetragonal, transformation toughened zirconia (3Y-TZP).

Prime Features:

  • Very high mechanical strength
  • Excellent wear and abrasion resistance
  • High impact resistance and toughness
  • Good thermal shock resistance
Typical Applications:
  • Typically used for blades and cutting edges where the fine grain structure is an advantageous
  • Gas and Oil field applications
  • Pump and Valve components
  • Canning and Metal Packaging
  • Solids Handling. Automotive (eg Weld Pins)
Production Capabilities:
  • Sintered components
  • Precision ground components
  • Ceramic / Metal assemblies
  • Ceramic design assistance

Information provided by Morgan Advanced Materials

Key Words: Nilcra ®
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.05 g/cc
@Temperature 20.0 °C
Grain Size 0.40 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 1250
@Temperature 20.0 °C
[kg/mm2], HV0.3
Modulus of Elasticity 205 GPa
@Temperature 20.0 °C
Flexural Strength 1000 MPa
@Temperature 20.0 °C
4pt bend
Compressive Strength 2300 MPa
@Temperature 20.0 °C
Poissons Ratio 0.30
@Temperature 20.0 °C
Fracture Toughness 8.00 MPa-m½
@Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+11 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µm/m-°C
@Temperature 24.0 - 400 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 3.00 W/m-K
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Y2O3 5.2 %in ZrO2
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade
Morgan Advanced Ceramics CIM Zirconia Technical Ceramic
Morgan Advanced Ceramics Nilcra® Zirconia HIP'ed 3Y-TZP Grade Y-TZP
Overview of materials for Nylon 12
Steatite (Magnesium Silicon Oxide)

CMORF5079 / 200317

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.