MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Petropol Makropol® B3 HV UV CRLA010 PC341 PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: Polycarbonate crystal, high viscosity, UV stabilized, excellent thermal and mechanical properties. Suitable for extrusion of multi wall sheet/profile.

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Water Absorption 0.12 %Humidity Absorption; ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 2577
Melt Flow >= 6.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 65.0 MPa50 mm/min; ISO 527-1/-2
Tensile Strength, Yield 67.0 MPa50 mm/min; ISO 527-1/-2
Elongation at Break 100 %50 mm/min; ISO 527-1/-2
Elongation at Yield 6.5 %50 mm/min; ISO 527-1/-2
Tensile Modulus 2400 MPa1 mm/min; ISO 527-1/-2
Flexural Strength 100 MPa2 mm/min; ISO 178
Flexural Modulus 2400 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 80.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 14.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 70.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Tensile Creep Modulus, 1 hour 2200 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 1900 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.650 µm/m-°CISO 11359-1,-2
Thermal Conductivity 0.200 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 137 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 126 °CISO 75-1,-2
Vicat Softening Point 144 °C
@Load 5.10 kg
50 °C/h; ISO 306
 145 °C
@Load 5.10 kg
120 °C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.750 mm
Glow Wire Test 850 °C
@Thickness 2.00 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Optical PropertiesOriginal ValueComments
Haze >= 0.80 %
@Thickness 3.00 mm
ISO 14782
Transmission, Visible >= 87 %
@Thickness 4.00 mm
ISO 13468-2
 89 %
@Thickness 2.00 mm
ISO 13468-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 - 300 °CMolding
Mold Temperature 60.0 - 100 °C
Drying Temperature 120 °C
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPETROPOL052 / 312960

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.