MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Krytox™ GPL 577 PFPE Grease
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Krytox™ GPL 577 is formulated with a high-viscosity base oil and special additives. This results in a grease that can withstand extreme conditions of temperature and load. The high viscosity of the base oil combined with the additives yields a product that is able to maintain a good lubricating film in very slow speed or high load applications. The high base oil viscosity also results in a grease that evaporates very slowly under conditions of high vacuum or temperature. Like all standard Krytox™ products, Krytox™ GPL 577 is nonflammable and compatible with oxygen, and will not react with most chemicals.

Information provided by Chemours Krytox

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.95 g/ccoil
Volatiles <= 1.0 %
@Treatment Temp. 99.0 °C,
Time 79200 sec
D972, modified
Viscosity Measurement 149Viscosity Index
Viscosity Measure 500 cSt
@Temperature 40.0 °C
oil
 
Mechanical PropertiesOriginal ValueComments
Penetration 265 - 295
Oil Separation <= 1.5 %
@Treatment Temp. 99.0 °C,
Time 108000 sec
FTMS 791B 321.1
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °C
Minimum Service Temperature, Air 35.0 °C
Pour Point -25.0 °C
 
Descriptive Properties
Grease 4 Ball Wear Test0.12ASTM D4172: 107 °C, 20 kg, 1200 rpm, 60 min. Friction Coefficient (0.003).
 0.6ASTM D4172: 107 °C, 20 kg, 1200 rpm, 60 min. Wear Scar, mm (0.01).
Mechanical Stability< 330100,000 times

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDUPJ850 / 254038

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.