MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Starflam® AFR450X2 PA66-GF25 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Starflam AFR450X2 is a glass filled, red phosphorous flame retardant PA66 for injection molded applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccDAM; ISO 1183
Water Absorption 1.0 %
@Temperature 23.0 °C,
Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.7 %
@Temperature 23.0 °C
DAM; ISO 62
Water Absorption at Saturation 6.0 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 90.0 MPa50% RH; ISO 527-2
 139 MPaDAM; ISO 527-2
Elongation at Break 2.6 %DAM; ISO 527-2
 4.8 %50% RH; ISO 527-2
Tensile Modulus 5600 MPa50% RH; ISO 527-2
 8600 MPaDAM; ISO 527-2
Flexural Strength 119 MPa50% RH; ISO 178
 203 MPaDAM; ISO 178
Flexural Modulus 5100 MPa50% RH; ISO 178
 8200 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 6.70 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 7.30 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 7.30 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 7.40 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 9.70 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 13.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 57.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 58.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 58.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 60.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 67.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 72.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 7.30 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 7.70 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 7.80 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 14.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
@Thickness 1.00 mm
DAM; IEC 60093
Surface Resistance 1.00e+16 ohm
@Thickness 1.00 mm
DAM; IEC 62631-3-2
Dielectric Strength 22.0 kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
 24.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
High Voltage Arc Resistance to Ignition (HVAR) >= 120 sec
@Thickness 0.750 mm
UL 746
 >= 120 sec
@Thickness 1.50 mm
UL 746
 >= 120 sec
@Thickness 3.00 mm
UL 746
Comparative Tracking Index <= 600 V
@Thickness 3.00 mm
IEC 60112
 >= 600 V
@Thickness 3.00 mm
IEC 60112
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.750 mm
UL 746
 >= 120 arcs
@Thickness 1.50 mm
UL 746
 >= 120 arcs
@Thickness 3.00 mm
UL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 28.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 261 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 256 °CUnannealed; 50% RH; ISO 75-2/B
 258 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 225 °CUnannealed; 50% RH; ISO 75-2/A
 239 °CUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical 110 °C
@Thickness 0.750 mm
UL 746
 110 °C
@Thickness 1.50 mm
UL 746
 110 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 110 °C
@Thickness 0.750 mm
UL 746
 110 °C
@Thickness 1.50 mm
UL 746
 110 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 115 °C
@Thickness 0.750 mm
UL 746
 115 °C
@Thickness 1.50 mm
UL 746
 120 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-2
@Thickness 0.750 mm
UL 94
 V-0
@Thickness 1.50 mm
UL 94
 V-0
@Thickness 3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature >= 275 °CInjection
 <= 285 °CInjection
Middle Barrel Temperature >= 275 °CInjection
 <= 285 °CInjection
Front Barrel Temperature >= 270 °CInjection
 <= 285 °CInjection
Melt Temperature >= 275 °CInjection
 <= 285 °CInjection
Mold Temperature >= 60.0 °CInjection
 <= 90.0 °CInjection
Drying Temperature >= 75.0 °CInjection
 <= 85.0 °CInjection
Dry Time 4.00 hourInjection
Moisture Content 0.10 %Injection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Release agent
AppearanceNatural Color
FeaturesFlame Retardant
 Halogen Content, None
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9115 / 287566

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.