Description: DA 4518 is an epoxy prepreg designed for a temperature range of -67°F (-55°C) to 350°F (177°C), with a cure of 250°F (121°C) for one hour and or a cure of 350º F (177ºC) for 1 hour. This material needs to be post cure or cured to 350ºF to get the 350º properties Mechanical Properties: The data supplied are averages obtained on 12 plies of DA 4518 on 7781 glass cured one hour at 250°F (121°C) with a heat up rate of 5° per minute from room temperature. Information provided by Adhesive Prepegs for Composite Manufacturers, LLC |