Celanex 3318 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is well suited for electrical connector applications. To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less than 0.02%. Drying should be done in a dehumidifying hopper dryer capable of dewpoints <-40°F (-40°C) at 250°F (121°C) for 4 hours. For subsequent storage of the material in the dryer until processed (<= 60 h) it is necessary to lower the temperature to 100° C.Information provided by Celanese Corporation. |
30% glass filled flame retardant PBT |